Sample VT400 °C exhibits a far more uniform particle size distribution and pores with an average grain dimension of about twelve nm (In keeping with ImageJ application Evaluation). However, altering deposition temperature to 700 °C larger and denser particles with a mean grain size of 460 nm was acquired. Sample VT400 Conversely includes a pa